Silicon nitride powders were prepared by the simultaneous reduction and nitridation from powder mixtures of Kim cheon quartzite and carbon (graphite or carbon black) at1400$^{\circ}C$ for 10 hours in nitrogen atmosphere. The effects of the reaction variables on the yield of products and on the ${\alpha}$/${\beta}$ ratio were examined. The average particle size, density, and the ${\alpha}$/${\beta}$ ratio of the obtained si3N4 were 1.0$\mu\textrm{m}$, 3.10g/㎤ and 90/10, respectively. It was found that the Si3N4 powders obtained in this work were comparable to the foreign commercial products.