Cement is the most widely used but generates a lot of CO₂, so we need a material to replace it. Using industrial by-products such as Silica Fume(SF), Blast furnace Slag(BS) and Fly Ash(FA) bring some advantages including CO₂ reduction and resource recycling. However, there is a limit to improve performance when using only one material. Therefore, the synergy effects of No cement binary mortar and ternary mortar were analyzed and compared. As a result, No cement ternary mortar had the strength higher than binary mortar. among ternary mortars, the specimen mixed 50% of BS had the highest strength. However, when SF was mixed by 20%, the flowability reduces. so 10% of SF, 40% of FA and 50% of BS is considered as the optimal mixing ratio.