견 피브로인의 알칼리 가수분해
Hydrolysis of Silk Fibroin on Alkali Conditions
김남정(Nam Jung Kim),배도규(Do Gyu Bae)
UCI I410-ECN-0102-2009-520-003959190

To hydrolyze silk fibroin was treated with NaOH solution on various concentrations and times. And it was examined that the addition effects of NaHS03 in NaOH solution on the solubility and colouring of silk fibroin. As obtained results are as follows; The more increasement of concentration and time of NaOH treatment, the more increasement of solubility but solubility was slight above 3% concentration of NaOH. Fibroin yield was decreased above 3% concentration. This was due to formation of peptide or amino acids below molecular weight 3,000. Most of molecular weight distribution came out to be under 3,000 in 2% concentration and 4hrs of NaOH treatment. The more increasement of adding concentration of NaHSO3, the more reduction of solubility but white index of powder increased. In the results of FT-IR spectras of silk fibroin powder obtained by various concentrations of NaHSO3 treatment, the absorbent peak at 3,400 cm-1 which was considered as -CH=N- (azo-methine) was disappeared by the more addition of NaHS0O3. It showed that absorbent peak of ß-fibroin moved into low temperature region and transferred to α- and random coil structure through the DSC experiment. In the results of amino acid analysis, alkali hydrolysis reduced the oxy amino contents acid like serine and tyrosine, but increased the glycine content by the more addition of NaHSO3.

[자료제공 : 네이버학술정보]
×